Quality control for sintered parts does not work like machining. Batches are large, cost pressure is real, and dimensions are set by both the die and the furnace. The effort goes into first-article approval, in-process sampling and the dimensions that matter.

Quality control for sintered parts follows a different logic from machining. A machined part comes off the machine one at a time and can be measured one at a time. Sintering loads hundreds or thousands of parts into a furnace at once, and every dimension is shaped by the die condition, the position in the load and the temperature distribution in the furnace. The point is not to measure everything, but to put the measurements where problems show up first.

The first gate is first-article approval. After a new die, a die repair or a change of powder lot, the first part is measured across the full drawing — CMM and vision system against gear form, span measurement over pins, hole positions, parallelism. This establishes the baseline for every sample that follows: die wear is gradual, and only with first-article data in hand can you tell whether a dimension is inside normal wear or has gone wrong.

The second gate is in-process sampling, at a frequency set by batch size and history, covering the critical and mating dimensions on the drawing. Dimensional variation in sintered parts comes from three main sources: fluctuation in apparent density and compacting pressure, progressive die wear, and differences in furnace zone temperatures and push rate. Data that drifts in one direction usually means the die is wearing; data that scatters up and down points to the furnace or the powder lot.

The third gate is density and hardness. Density is measured by the Archimedes method and is the most direct indicator of whether sintering was complete. Hardness follows the drawing, Rockwell or Vickers, with the caveat that porosity distorts the indentation — so the test location, load and scale all belong in the technical agreement. Density and hardness both running low usually means the sintering temperature or hold time was insufficient.

The fourth gate is appearance and defects. The usual suspects are chipped corners, cracks, laminations, ejection marks and uneven oxidation colour, most of them created during compaction or sintering. On high-volume parts, automatic optical sorting equipment screens by dimension and appearance first, pulling out the obvious rejects, and the borderline parts go to manual inspection. Such equipment cannot replace human judgement, but it keeps the large majority of clear defects from ever reaching a customer.

The fifth gate is mechanical testing and metallography, as required. Gears are commonly checked for radial crushing strength; oil-impregnated bearings for oil content and crushing strength; and where specified, a cross-section is examined for pore morphology, the pearlite-to-ferrite ratio and case depth — all of which reflect back on process stability.

The step where things most often go wrong is not inspection itself but an acceptance standard left unwritten. How density is measured, which hardness scale applies, and how much of a surface defect is still acceptable: without agreement on those three, nearly every dispute at shipment starts here. We recommend fixing appearance with limit samples agreed together with the customer at the sampling stage.

Our practice is to keep inspection records for every batch, with density, hardness and critical dimensions traceable alongside the goods — and, where a customer requires it, back to the specific furnace run and die number.

If a part has critical dimensions or special acceptance requirements, state them when you send the drawing, and we will include the inspection plan and acceptance criteria in the quotation.