'Density not below 6.6 g/cm³' is not a decorative note on a drawing — it sets strength, hardness and wear resistance. Understanding how density, porosity and mechanical properties relate is the first step to reading a sintered part correctly.
Sintered part drawings often carry an unremarkable line — density not below a certain value, say 6.6 g/cm³. Many buyers treat it as an optional target. In practice, it decides whether the part works at all.
The reasoning is straightforward. A sintered part is not fully dense metal; it retains a proportion of porosity. Higher density means less porosity and more complete metallurgical bonding between particles, so the part approaches the mechanical properties of a forging. Lower density means more porosity, and strength, hardness and fatigue life all drop noticeably.
The industry usually bands sintered steel by density. Below 6.0 g/cm³ is considered low density, used for structural parts with modest strength requirements. From 6.0 to 6.8 g/cm³ is the general-purpose middle band, covering most gears, bushings and structural parts. Above 6.8 g/cm³ is high density, where strength and wear resistance approach medium-carbon steel and the parts are used in drives under real load.
So 6.6 g/cm³ is not an arbitrary figure. It sits at an economical, sufficient point: enough strength for ordinary transmission parts without paying the cost of chasing higher density.
One caveat: density is not uniform. Within a single part, density at the rim and in thin walls is usually higher than in the centre of a thick section, because powder fills and compacts differently inside the die. The thicker and more complex the part, the larger that spread. If the critical load path runs through a thick section, the average density on the drawing is not enough information — the design stage has to account for it.
If higher strength really is needed, there are three routes: raise density (adjust the material mix, increase compaction pressure, or move to warm compaction), add a heat treatment, or move to a higher-tier process such as sinter forging. All three raise cost, so the more common answer is to establish the actual load and life requirement during design and set the density target where it is just sufficient.
Density also affects downstream processing. Higher-density parts respond better to hardening and carburising. Lower-density parts tend to trap plating or blackening solutions in the porosity and need an additional sealing step.
When you see a density requirement, the right move is not to copy it forward but to confirm the real load and life of the part, and then decide whether that number can be relaxed.