A quoted ±0.01 mm means very different things depending on whether the dimension comes from the die or from a later sizing or grinding step. Separating the two avoids most incoming-inspection disputes.
A quotation says ±0.01 mm. The instinctive question is whether that can be held. The more useful question is where that dimension comes from. On a sintered part, tolerances fall into two families: those the die holds directly, and those a later operation produces. Their difficulty and cost are very different.
Die-held dimensions are fixed by geometry at compaction. Tooth form, bore size, concentricity and similar features carry the same precision on every part as soon as the die cavity is correct. Repeatability is excellent, and this is the core value of powder metallurgy: the precision of the tooling replaces per-piece cutting time.
But there is a ceiling. Because compaction is directional and powder has to fill the die, tolerances a die can hold reliably usually sit around ±0.02 to ±0.05 mm, depending on feature size, wall uniformity and material. Larger and more asymmetric parts are harder to hold.
To go beyond that ceiling requires secondary operations: sizing, grinding, turning, reaming. These can reach ±0.005 mm or tighter, but each added operation costs money and lead time and erodes the very advantage of net-shape forming.
At drawing review, then, it is worth walking through the critical dimensions: which ones genuinely affect assembly and service life, and which are marked out of habit. The genuinely critical ones should be assigned to a specific operation. The rest can be relaxed into the band the die holds comfortably. That alone often lowers unit price without changing performance.
A few dimensions deserve particular attention. Bore and shaft fits are usually the target of secondary operations. Tooth accuracy is driven by the die and is hard to improve afterwards. Face parallelism and flatness rely on a combination of compaction and sizing.
One more point that is often missed: tolerances have to leave room for sintering shrinkage. Parts shrink during sintering by a material-specific factor, and the die cavity is cut oversize to compensate. If the tolerance band on the drawing is narrower than the natural variation of that shrinkage, the requirement is not process-capable and needs to be discussed up front.
In practice we give tolerance feedback against the drawing before quoting: what can be held directly, what needs a secondary operation, and what should be renegotiated with the designer. Settling that first is far cheaper than discovering it after a production run.