Tooth breakage, pitting, wear and noise usually trace back to choices made on the drawing. Working backwards from failure mode to design rule costs far less than reworking a part in the field.

When a small gear fails at the customer, the cause is usually not a drifting production batch but a decision taken at design. The four modes below cover most field complaints.

The first is tooth breakage. The tooth root is where stress concentrates hardest. If the root fillet is too small, or the load was underestimated, the root cracks first. In sintered parts root strength also depends on density: at insufficient density even a generously designed root may not hold. The countermeasures are a proper root fillet, a controlled density target, and heat treatment where needed.

The second is pitting. This is contact fatigue: fine pits appear on the flank after repeated loading and grow into craters. It usually means contact stress exceeds the fatigue limit of the material, or that flank hardness and lubrication are inadequate. The answer is to reduce contact stress — larger module, wider face — or raise flank hardness.

The third is wear. Wear shows up as steadily thinning teeth and a distorted profile. Because sintered parts contain porosity, their wear resistance is inherently below that of fully dense steel, which makes dusty environments and poor lubrication worse. Higher density, surface densification or oil impregnation all improve it.

The fourth is noise. Noise is not a failure itself but a signal pointing to tooth form error, centre distance deviation or concentricity problems. Tooth accuracy in a sintered part comes from the die, so once the die wears or the design under-specifies tooth control, noise rises. Investigation should focus on die condition and assembly datums.

All four share one thing: their root causes can mostly be designed out rather than compensated for in production. The more effective route is to state the operating conditions before the drawing is fixed — load, speed, shock, lubrication and expected life. That information determines whether the part survives far more than dimensional tolerances do.

If a failure has already happened, send the failed part together with the installation conditions and we can usually form an initial view. Where there is a fracture, the fracture surface itself is a fairly direct clue.